Flexural Modulus

Flexural modulus is a plastic's stiffness measured in bending on a molded bar under ISO 178, printed in MPa. Datasheets print it beside tensile modulus.

Every Flexural Modulus article of the Injection Molding Resources, newest first, each written from published standards, research and makers’ data.

Meaning

Flexural modulus is a plastic’s stiffness measured in bending on a molded bar under ISO 178, printed in MPa. Datasheets print it beside tensile modulus. For nylon it falls sharply once the part takes up water.

Values

Zytel 70G33HS1L glass nylon reads 9,500 MPa (1.38 million psi) dry and 6,000 MPa (870,000 psi) conditioned. That is a loss of 37 percent from water alone. Makrolon 2407 polycarbonate reads 2,350 MPa (341,000 psi), with a flexural strength of 98 MPa (14,200 psi). Delrin 500P acetal reads 3,000 MPa (435,000 psi). Covestro measures its value under ISO 178 at 23 °C and 50 percent relative humidity.
Read More

Moisture

The nylon figure falls more than tensile stress or flexural stress do. Flexural stress drops 31 percent, from 290 to 200 MPa. Quoting the dry figure alone describes a part that changes before assembly.

Glass Fiber Length

In glass-reinforced nylon 66, stiffness depends on how long the fibers stay through molding. DuPont charts retained flexural modulus, tensile strength and impact strength against rear zone temperature. The retained share falls as the rear zone is set cooler. The guide proposes a rear zone of at least 290 °C for glass-reinforced nylon 66, and the largest loss is in impact.

Temperature

The Zytel sheet carries stress-strain and secant modulus curves from -40 to 149 °C (-40 to 300 °F). Stiffness falls as the part warms toward its glass transition at 80 °C (176 °F). A bending test at 23 °C says little about a cover that sits at 80 °C beside a motor.

Drying Resin and Setting Melt Temperature Before the First Injection Molded Part

Pellets are dried to a measured moisture limit, held there to the hopper, and melted inside a window that the resin maker prints.

What Dry Resin and a Correct Melt Temperature ProtectWater in a nylon melt is not a surface problem. DuPont explains that water carried into the melt triggers hydrolysis, which breaks the polymer down, costs toughness and strength, and makes the melt flow more easily.

Polycarbonate Injection Molding Properties for Clear and Tough Parts

Polycarbonate read from the maker's sheets for a buyer: what it molds like when dry and hot, how thin walls fill, and what to ask of an aluminum tool.

Makrolon 2407 Properties in Metric and Inch UnitsMakrolon 2407 is a low-viscosity, general-purpose, UV-stabilized, easy-release polycarbonate with a melt volume-flow rate of 19 cm³/10 min at 300 °C and 1.2 kg under ISO 1133. Its ISO short name is ISO 7391-PC,MLR,(,,)-18-9.

Glass-Filled Nylon 66 in Injection Molding and What It Does to an Aluminum Tool

How a glass-reinforced nylon behaves dry and conditioned, in the press and on an aluminum tool, and what its datasheet leaves for the buyer to settle.

Properties of 30 Percent Glass-Filled Nylon 66 Dry and ConditionedPA66 with 30 percent glass is one of the most common reinforced engineering grades, and BASF's Ultramid A3WG6 LT BK, a laser-transparent black grade whose sheet is dated 09/2026, is a clear example of how the family reads. The sheet names the polymer PA66-GF30 and gives its typical values for uncolored product at 23 °C.

Request an Injection Molding Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Injection Molding chosen.

Request a Quote