Coating

A mold coating is a thin hard layer on an aluminum cavity, nickel-boron of 5 to 8 µm here, that resists wear.

Every Coating article of the Injection Molding Resources, newest first, each written from published standards, research and makers’ data.

Meaning

A mold coating is a thin hard layer on an aluminum cavity, nickel-boron of 5 to 8 µm here, that resists wear. A Plastics Technology article on aluminum tools gives the figures. The coating raises the surface to 50 to 56 HRC. It also reduces oxidation and acts as a release agent.

Application

The nickel-boron coat is about 5 to 8 µm (0.0002 to 0.0003 in) thick. It takes about three days to apply. When it wears it can be stripped and recoated. The same article describes a four-cavity ABS tool near 200,000 shots whose hard coat was stripped and reapplied midstream. That happened when a logo was removed by machining and welding, and the surface was polished again after the weld.
Read More

Placement

Filled resins wear the shutoffs and the gate area first. The coating is one remedy, and steel inserts at the high-wear areas are the other. Acetal carries no glass, so abrasive wear is not its first concern.

Coating and Finish

A coat of 5 to 8 µm is several hundred times the Ra of an SPI A-1 surface. It is thicker than every polished and paper grade is rough. The finish a part shows is therefore the finish of the coated surface. A polish applied under the coating and one applied over it give different surfaces, so the order is agreed with the toolmaker.

Upkeep

The tool is checked for wear and galling every time it leaves the press. A cosmetic finish on a coated tool is maintained, and the plan says whether it is restored at cleaning or only inspected.

Mold Maintenance and Spare Inserts Across a Bridge Injection Molding Run

How a bridge mold is cleaned, inspected and fitted with inserts across a run, so that wear is recorded, predicted and met with spares instead of stoppages.

What a Bridge Mold Needs Between LotsThe aluminum maintenance column is plain on the first rule: an aluminum mold is taken apart and cleaned thoroughly after every run of parts, and cleaned again before storage, however short the run. It can often run five to seven days before it needs cleaning, the author notes, though some resins and some molds with actions need it after two to three days.

Draft Angle by Texture Depth on Injection Molded Parts

How much draft a textured wall needs for its depth, under which conditions each published figure holds, and how the mold and the part are checked.

How Much Draft a Texture Depth NeedsStandex Engraving Mold-Tech's technical data sheet gives the current recommendation from the texture maker: 1° of draft for every 0.013 to 0.015 mm (0.0005 to 0.0006 in) of texture depth. Per 0.025 mm (0.001 in) that works out to between 1.7° and 2°.

How Tightly Acetal Parts Hold Dimension in Injection Molding

Acetal dimension spread measured on one part under four press settings, with the gate and cooling rules behind it and a tolerance budget for a 50 mm feature.

Outer Diameter Spread Under Four Packing and Cooling SettingsThe test part in DuPont's tips is a tribological sample used for wear and friction testing, a part whose outer diameter has to be as dimensionally precise as possible. DuPont molded it under four settings, measured the outer diameter and reported the mean with its variation.

SPI Mold Finish Grades A-1 to D-3 for Injection Molded Parts

The SPI finish grades read for a buyer, with what each method gives, how texture costs draft, and how a finish is written and kept on an aluminum tool.

What the Twelve SPI Finish Grades SpecifyThe SPI system names a finish by a letter and a number. Its letter gives the finishing method, A for diamond buff, B for grit paper, C for stone and D for dry blast, while the number runs from 1, the finest within a letter, to 3, the coarsest.

Glass-Filled Nylon 66 in Injection Molding and What It Does to an Aluminum Tool

How a glass-reinforced nylon behaves dry and conditioned, in the press and on an aluminum tool, and what its datasheet leaves for the buyer to settle.

Properties of 30 Percent Glass-Filled Nylon 66 Dry and ConditionedPA66 with 30 percent glass is one of the most common reinforced engineering grades, and BASF's Ultramid A3WG6 LT BK, a laser-transparent black grade whose sheet is dated 09/2026, is a clear example of how the family reads. The sheet names the polymer PA66-GF30 and gives its typical values for uncolored product at 23 °C.

Request an Injection Molding Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Injection Molding chosen.

Request a Quote