Cavity

The cavity is the hollow in a mold that gives a molded part its shape, cut larger than the part by the resin's shrinkage.

Every Cavity article of the Injection Molding Resources, newest first, each written from published standards, research and makers’ data.

Meaning

The cavity is the hollow in a mold that gives a molded part its shape, cut larger than the part by the resin’s shrinkage. A tool can carry one cavity or several, and each forms a part with every shot. The part copies the cavity surface, and the cavity walls hold the part while it cools. Most corrections a bridge run needs end as a few tenths of a millimeter cut into the cavity.

Cavity Dimension

A toolmaker cuts the cavity to the part dimension divided by one minus the shrinkage fraction. For polycarbonate at 0.6 percent, a 100 mm (3.94 in) part needs a 100.60 mm cavity. Glass-filled nylon 66 needs 100.30 mm along the flow and 101.11 mm across it. Acetal needs 102.04 mm along the flow. One allowance cut for a whole glass nylon part is wrong in one direction by 0.8 mm per 100 mm.
Read More

Effect on Hours

Parts per hour equal 3,600 divided by the cycle in seconds, times the cavity count, at full uptime. At a 26 second cycle, 5,000 parts need about 36 hours with one cavity. With four cavities they need about 9 hours. More cavities also ask for more clamp force and a bigger shot. A 600 kN (65 ton) press at 90 MPa (13,050 psi) holds about 6,700 mm² (10.3 in²) of projected area. That figure includes the runner and is an upper bound. Real cavity pressure sits below the pressure at the screw, so flow analysis sets the final number.

Cooling and Release

A part left in the cavity is held by the walls and cores while it shrinks. DuPont’s acetal test part shows the cost of that hold. Cooling 15 seconds in the mold after full packing widened the spread of its 49.6 mm (1.95 in) diameter. The spread went from ±0.02 mm to ±0.07 mm. Acetal is therefore ejected hot and cooled in air, where it shrinks without constraint. A part has to leave the cavity on the intended side. One that sticks to the cavity half instead of the core points to draft, polish or temperature. DuPont recommends 0.5° to 1° of draft per side for nylon, and up to 2° for softer, more elastic resins. Covestro suggests different temperatures on the two mold halves to hold the part on the chosen side.

Correction

DuPont corrects the cavity only after the gate and the process have been checked. It never compromises the process settings to hit a dimension. An aluminum cavity can be recut, welded or enlarged after the first samples. That is the practical reason a bridge tool is made of it. A second sample confirms the correction, and the approved sample becomes the reference for the run. A first sample measured 10 °C warm misleads the correction, and the cavity ends up too small.

Surface and Wear

The molded surface copies the cavity surface, so a clear part is only as clear as the polish it met. The SPI grades name that finish, from A-1 at an Ra of 0.012 to 0.025 µm to D-3 at 3.2 to 18 µm. A nickel-boron coating of 5 to 8 µm (0.0002 to 0.0003 in) is thicker than every polished grade is rough. The order of polishing and coating is therefore agreed with the toolmaker. Galling from excessive temperature and injection pressure damages the cavity surface, and every later part copies the damage. Each cavity wears with every shot. A dimension that moves one way across successive lots is the usual sign of a cavity or core wearing away. Cavities and runners are vented at the parting line and at the ejectors. A vent that clogs shows as a burn mark at the end of flow.

Sampling by Cavity

ISO 2859-1 calls for a stratified sample when a lot divides into sensible sub-lots. Each cavity of a multi-cavity tool is such a stratum, so the sample is drawn across the cavities in proportion. The cavity is marked on the part, or the sample cannot be stratified. A first article records the cavity each measured part came from.

Mold Maintenance and Spare Inserts Across a Bridge Injection Molding Run

How a bridge mold is cleaned, inspected and fitted with inserts across a run, so that wear is recorded, predicted and met with spares instead of stoppages.

What a Bridge Mold Needs Between LotsThe aluminum maintenance column is plain on the first rule: an aluminum mold is taken apart and cleaned thoroughly after every run of parts, and cleaned again before storage, however short the run. It can often run five to seven days before it needs cleaning, the author notes, though some resins and some molds with actions need it after two to three days.

Short Shot, Sink and Flash in Injection Molding Traced to Their Cause

Short shots, sinks and flash traced to the melt volume, pressure and steel behind them, with the checks that find the cause before a setting is moved.

What Short Shots, Sink and Flash Have in CommonA short shot is a part the cavity never finished. BASF's troubleshooting brochure for engineering thermoplastics describes it as a part not completely formed, mainly in the areas furthest from the gate or in thin walls.

Gate Location and Gate Freeze in Injection Molding

Where a gate goes, how big it is and how long it stays open, with the weight study that sets hold time from the gate itself.

How Gate Location and Gate Freeze Shape a Molded PartAutodesk's Moldflow design rules open with the claim that gate position strongly affects material orientation and warpage, and that changing the gate is sometimes the only way to control orientation. Every gate injects under the same pressure, and the aim of gating is to avoid overpacking some paths while others are still filling, because unequal packing gives unequal shrinkage.

Draft Angle by Texture Depth on Injection Molded Parts

How much draft a textured wall needs for its depth, under which conditions each published figure holds, and how the mold and the part are checked.

How Much Draft a Texture Depth NeedsStandex Engraving Mold-Tech's technical data sheet gives the current recommendation from the texture maker: 1° of draft for every 0.013 to 0.015 mm (0.0005 to 0.0006 in) of texture depth. Per 0.025 mm (0.001 in) that works out to between 1.7° and 2°.

Polypropylene for Living Hinges in Injection Molding

Polypropylene for living hinges read from design guides and molding columns: grade choice, hinge dimensions, gating across the web, cooling and the tests that prove a hinge.

Why Polypropylene Makes a Living HingeThe MIT design note explains the mechanism. When a partly oriented polypropylene web is cold drawn on its first flex, it stretches by ratios of 2 or 3 to 1, and its tensile strength rises sharply.

ABS and PC/ABS Blends in Injection Molding

ABS and PC/ABS read from the makers' datasheets: drying, processing windows, shrinkage, snap-fit strain, impact and when the blend earns its stricter dryer.

How ABS and PC/ABS Differ in Injection MoldingABS is a terpolymer, and Moldflow's material page describes its structure: a continuous phase of styrene-acrylonitrile with a dispersed phase of polybutadiene rubber. Acrylonitrile brings hardness and chemical and heat resistance, styrene brings processability, gloss and strength, and butadiene brings toughness and impact strength.

How Many Parts One Aluminum Injection Mold Gives

A mold's life is a toolmaker's rating for a stated resin and cavity count, converted into parts per tool and then into tools per quantity.

What Sets the Number of Parts One Aluminum Mold GivesThree things set it, and they act together. One is the alloy and where in the plate the cavity sits.

Cycle Time and Parts per Hour in a Bridge Injection Molding Run

A cycle is the sum of fill, hold, cooling and press motions, and a supplier's number is only as good as the pack and cooling times behind it.

What Sets Cycle Time and Parts per HourA molding cycle is a loop of seven moves: the mold closes, the cavity fills, the pack and hold phase runs, the part cools, the mold opens, the part is ejected, and the screw recovers for the next shot. Recovery runs while the part cools, which is why DuPont's nylon guide asks for screw speeds adjusted so that screw retraction time is shorter than the cooling phase.

How to Start Up an Injection Mold and Take the First Shots

A new mold is started cold on purpose, filled in stages with short shots, and read for vents, gates and heat before any process is fixed.

The Start-Up Sequence from a Cold Barrel to the First ShotEight moves take a machine from cold to its first complete part. The first four prepare the melt, the next three shape the shot, and the last one is a decision: whether the part describes the tool or only the settings.

How Temperature Changes the Size of a Molded Plastic Part at the Gauge

How coefficients of expansion turn a few degrees of gauge temperature into hundredths of a millimeter, by resin and direction, and what a drawing should state.

Linear Thermal Expansion of Polycarbonate, Glass-Filled Nylon and AcetalLinear thermal expansion is reported on datasheets as a coefficient, the length change per unit length per degree. The three makers print it by the ISO or TMA method, and they differ in how finely they split it.

Injection Molding Shrinkage Along and Across the Flow by Material

Molding shrinkage read by direction and condition for three resins, with the process settings that move it and the way a first sample turns it into a cavity allowance.

Shrinkage of Polycarbonate, Glass-Filled Nylon 66 and Acetal Along and Across the FlowISO 294-4:2018 sets out the method for measuring mold shrinkage and post-mold shrinkage of injection molded thermoplastic test specimens, parallel and normal to the direction of melt flow. Resin makers print the result in two lines, one per direction.

How Tightly Acetal Parts Hold Dimension in Injection Molding

Acetal dimension spread measured on one part under four press settings, with the gate and cooling rules behind it and a tolerance budget for a 50 mm feature.

Outer Diameter Spread Under Four Packing and Cooling SettingsThe test part in DuPont's tips is a tribological sample used for wear and friction testing, a part whose outer diameter has to be as dimensionally precise as possible. DuPont molded it under four settings, measured the outer diameter and reported the mean with its variation.

SPI Mold Finish Grades A-1 to D-3 for Injection Molded Parts

The SPI finish grades read for a buyer, with what each method gives, how texture costs draft, and how a finish is written and kept on an aluminum tool.

What the Twelve SPI Finish Grades SpecifyThe SPI system names a finish by a letter and a number. Its letter gives the finishing method, A for diamond buff, B for grit paper, C for stone and D for dry blast, while the number runs from 1, the finest within a letter, to 3, the coarsest.

ISO 20457 Tolerances for Plastic Molded Parts Read for the Buyer

How ISO 20457 is worded for plastic molded parts, what a supplier signs when a drawing cites it, and which items stay outside it for the order to settle.

What ISO 20457 Covers for Injection Molded PartsAccording to the abstract published by the Swedish Institute for Standards (SIS), ISO 20457 specifies possible manufacturing tolerances for plastic moulded parts, and it covers all integral features with general tolerances, using a surface profile tolerance within a specified datum system. It applies to injection moulding, injection compression moulding, transfer moulding, compression moulding and rotational moulding of non-porous parts in thermoplastics, thermoplastic elastomers and thermosets.

Request an Injection Molding Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Injection Molding chosen.