Cycle Time

Cycle time is the time from one shot to the next, the sum of mold closing, fill, pack and hold, cooling, opening and ejection.

Every Cycle Time article of the Injection Molding Resources, newest first, each written from published standards, research and makers’ data.

Meaning

Cycle time is the time from one shot to the next, the sum of mold closing, fill, pack and hold, cooling, opening and ejection. Screw recovery runs during cooling and adds nothing while it stays shorter. Cycle time turns a quantity into hours on a press. The same total can hide a tight process or a loose one.

Parts per Hour

One hour is 3,600 seconds, so shots per hour at full uptime are 3,600 divided by the cycle. Parts per hour are shots times the cavity count. Real uptime is lower, because the press stops for lot changes, inspections, purges and tool cleaning. A quoted figure says whether it is arithmetic or a measured run.
Read More

Trial Data

DuPont’s four acetal trials ran 39, 26, 26 and 41 seconds, or 92, 138, 138 and 88 shots an hour at one cavity. Trials 2 and 3 shared a 26 second cycle. Only trial 3 was good, with 15 seconds of packing and 2 of cooling. It held ±0.02 mm, while trial 2 varied by ±0.7 mm. Early ejection made trial 3 about 37 percent shorter than the 41 second trial with mold cooling.

Interval Owners

Fill and pack are set by the resin and the gate. Cooling is set by the wall, the resin and the tool metal. Opening, ejection and closing are set by the press and the part’s shape. The interval worth questioning is the one the part does not need. Extra cooling on a crystalline resin, or extra hold after gate freeze, adds seconds without quality.

Tool Metal

MoldMAX credits its copper alloys with cycles shorter by 15 to 50 percent. It prints 10 seconds of mold cooling against 25 seconds for its comparison tool. Those are the maker’s figures for its own alloys. When cycle time becomes the main variable in a program, a faster-cooling alloy is one reason for the next tool.

Quote Check

A buyer asks whether parts per hour assume full or measured uptime. The cavity count and the press behind the cycle come next. The pack and cooling times behind the total allow a check against a weight study. A cycle quoted before that study is an estimate. In a lot record, the cycle with its pack and cooling times shows whether the cycle was held.

Mold Maintenance and Spare Inserts Across a Bridge Injection Molding Run

How a bridge mold is cleaned, inspected and fitted with inserts across a run, so that wear is recorded, predicted and met with spares instead of stoppages.

What a Bridge Mold Needs Between LotsThe aluminum maintenance column is plain on the first rule: an aluminum mold is taken apart and cleaned thoroughly after every run of parts, and cleaned again before storage, however short the run. It can often run five to seven days before it needs cleaning, the author notes, though some resins and some molds with actions need it after two to three days.

Draft Angle by Texture Depth on Injection Molded Parts

How much draft a textured wall needs for its depth, under which conditions each published figure holds, and how the mold and the part are checked.

How Much Draft a Texture Depth NeedsStandex Engraving Mold-Tech's technical data sheet gives the current recommendation from the texture maker: 1° of draft for every 0.013 to 0.015 mm (0.0005 to 0.0006 in) of texture depth. Per 0.025 mm (0.001 in) that works out to between 1.7° and 2°.

How Many Parts One Aluminum Injection Mold Gives

A mold's life is a toolmaker's rating for a stated resin and cavity count, converted into parts per tool and then into tools per quantity.

What Sets the Number of Parts One Aluminum Mold GivesThree things set it, and they act together. One is the alloy and where in the plate the cavity sits.

Cycle Time and Parts per Hour in a Bridge Injection Molding Run

A cycle is the sum of fill, hold, cooling and press motions, and a supplier's number is only as good as the pack and cooling times behind it.

What Sets Cycle Time and Parts per HourA molding cycle is a loop of seven moves: the mold closes, the cavity fills, the pack and hold phase runs, the part cools, the mold opens, the part is ejected, and the screw recovers for the next shot. Recovery runs while the part cools, which is why DuPont's nylon guide asks for screw speeds adjusted so that screw retraction time is shorter than the cooling phase.

How Tightly Acetal Parts Hold Dimension in Injection Molding

Acetal dimension spread measured on one part under four press settings, with the gate and cooling rules behind it and a tolerance budget for a 50 mm feature.

Outer Diameter Spread Under Four Packing and Cooling SettingsThe test part in DuPont's tips is a tribological sample used for wear and friction testing, a part whose outer diameter has to be as dimensionally precise as possible. DuPont molded it under four settings, measured the outer diameter and reported the mean with its variation.

Request an Injection Molding Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Injection Molding chosen.

Request a Quote