Part Weight

Part weight is the weight of a molded part with runner and sprue removed, used to find the hold time and to watch a run.

Every Part Weight article of the Injection Molding Resources, newest first, each written from published standards, research and makers’ data.

Meaning

Part weight is the weight of a molded part with runner and sprue removed, used to find the hold time and to watch a run. A part that weighs less than its sister parts holds less plastic. It is more likely under-packed than mismeasured. Weighing takes a minute on a laboratory balance, which makes it the cheapest process record there is.

Weight Study

DuPont’s nylon guide gives the method. Total cycle time stays constant for the whole study, so that the melt temperature does not drift. Parts are molded at hold times 0.5 to 1.0 seconds apart, depending on the resolution wanted. Each part is weighed without its runner and sprue. Weight is then plotted against hold time. The right hold time is where the weight first stops rising. Shrinkage reaches its minimum at the same hold time, so a dimensional check on those parts confirms the reading. Beyond that point more hold adds nothing, because the gate has frozen, and it takes cycle time from the line. A weight that never reaches a plateau means the gate freezes before the part is packed. The correction then sits at the gate, not at the machine.
Read More

Acetal Case

DuPont’s Delrin tips show the same pattern on a wear-test part. An optimum packing time of 15 seconds gave the highest part weight and the least warpage. With 2 seconds of cooling that part held its 49.6 mm (1.95 in) diameter to ±0.02 mm. Trial 2 used the same 26 second cycle with 10 seconds of packing and varied by ±0.7 mm. The cycle did not change and the quality did.

Thickness Effect

Packing time does not scale in proportion to the wall. DuPont’s plot shows packing time per millimeter rising as thickness rises. The Delrin 500P sheet’s 8 s/mm is therefore an average, and thicker walls sit above it. A 2 mm rib and a 6 mm boss do not need three times the hold, because the thick section needs a disproportionate share. The optimum is found by weighing parts, not by reading one figure off a sheet.

Wear Gauge

A weight study repeated during a run becomes a wear gauge. A gate that wears larger changes the packing, so a mold can give a heavier or lighter part before its cavity shows visible damage. A gate, a shut-off or a check ring that has changed shows as weight drifting at a hold time that used to give a plateau. In a lot record, weight is the earliest sign of that change, long before a dimension leaves its limit.

Shrinkage Meter

Weight stands in for shrinkage on the press. A part from a short hold shrinks more, and its dimensions will not match later production parts. DuPont’s nylon guide sets the hold time where weight peaks because shrinkage is lowest there. A dimension controlled by weight is checked by weighing, which a toolroom does in a minute. A buyer reviewing first samples can ask for the plot of part weight against packing time. That plot shows the process was set before the cavity was touched. DuPont’s order of correction depends on it, because gate and process come before any cavity change. In a lot record, part weight at the set hold time shows whether the part is packed and the gate is behaving.

Record

A start-up adjusts first for appearance and then for maximum part weight. The pack time is then fixed by the weight study. A cycle quoted before that study is an estimate, and one quoted after it is a measurement. A shrinkage figure on a first sample counts only if its hold time sits on the plateau. The first-article record carries the hold time and the part weight at which the plateau was reached. Later lots are compared with that weight. A trial report that lists hold time without the weights behind it has skipped the measurement that makes the number repeatable. A lot whose weight holds the plateau is a lot packed the same way.

Short Shot, Sink and Flash in Injection Molding Traced to Their Cause

Short shots, sinks and flash traced to the melt volume, pressure and steel behind them, with the checks that find the cause before a setting is moved.

What Short Shots, Sink and Flash Have in CommonA short shot is a part the cavity never finished. BASF's troubleshooting brochure for engineering thermoplastics describes it as a part not completely formed, mainly in the areas furthest from the gate or in thin walls.

How Many Parts One Aluminum Injection Mold Gives

A mold's life is a toolmaker's rating for a stated resin and cavity count, converted into parts per tool and then into tools per quantity.

What Sets the Number of Parts One Aluminum Mold GivesThree things set it, and they act together. One is the alloy and where in the plate the cavity sits.

Cycle Time and Parts per Hour in a Bridge Injection Molding Run

A cycle is the sum of fill, hold, cooling and press motions, and a supplier's number is only as good as the pack and cooling times behind it.

What Sets Cycle Time and Parts per HourA molding cycle is a loop of seven moves: the mold closes, the cavity fills, the pack and hold phase runs, the part cools, the mold opens, the part is ejected, and the screw recovers for the next shot. Recovery runs while the part cools, which is why DuPont's nylon guide asks for screw speeds adjusted so that screw retraction time is shorter than the cooling phase.

How to Start Up an Injection Mold and Take the First Shots

A new mold is started cold on purpose, filled in stages with short shots, and read for vents, gates and heat before any process is fixed.

The Start-Up Sequence from a Cold Barrel to the First ShotEight moves take a machine from cold to its first complete part. The first four prepare the melt, the next three shape the shot, and the last one is a decision: whether the part describes the tool or only the settings.

Injection Molding Shrinkage Along and Across the Flow by Material

Molding shrinkage read by direction and condition for three resins, with the process settings that move it and the way a first sample turns it into a cavity allowance.

Shrinkage of Polycarbonate, Glass-Filled Nylon 66 and Acetal Along and Across the FlowISO 294-4:2018 sets out the method for measuring mold shrinkage and post-mold shrinkage of injection molded thermoplastic test specimens, parallel and normal to the direction of melt flow. Resin makers print the result in two lines, one per direction.

How Tightly Acetal Parts Hold Dimension in Injection Molding

Acetal dimension spread measured on one part under four press settings, with the gate and cooling rules behind it and a tolerance budget for a 50 mm feature.

Outer Diameter Spread Under Four Packing and Cooling SettingsThe test part in DuPont's tips is a tribological sample used for wear and friction testing, a part whose outer diameter has to be as dimensionally precise as possible. DuPont molded it under four settings, measured the outer diameter and reported the mean with its variation.

Request an Injection Molding Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Injection Molding chosen.

Request a Quote