Hot Runner

A hot runner is a heated manifold with nozzles that carries melt to the gates, so no runner is molded and cooled with each shot.

Every Hot Runner article of the Injection Molding Resources, newest first, each written from published standards, research and makers’ data.

Meaning

A hot runner is a heated manifold with nozzles that carries melt to the gates, so no runner is molded and cooled with each shot. It removes the runner from the cooling part of the cycle. It adds metal that has to be soaked, isolated and kept clean. In an aluminum tool it also adds an expansion problem.

Heat-Up

DuPont asks for the manifold to be brought to about 20 °C (35 °F) below the resin’s melting point. It is held there for at least 30 minutes before the final heat-up. Modern controllers can run that stepwise start automatically.
Read More

Aluminum Tool

Arconic states that hot runners can be integrated into QC-10 molds when the design allows for aluminum’s properties. Aluminum conducts heat 4 to 5 times as well as P-20, so the manifold is thermally isolated. A water-cooled hot half plate is the simplest method. Hardened steel inserts, sleeves, bushings or pads sit wherever the hot runner touches aluminum. They resist hobbing from the thrust pads, support ring, nozzle head, nozzle tip and inlet. Water-cooled gate inserts go with blind nozzle tips.

Expansion

QC-10 expands at 24.7 × 10⁻⁶ per K, about twice P-20. A 300 mm (11.8 in) plate heated through 40 K grows about 0.30 mm in QC-10 and 0.15 mm in P-20. Location and expansion dowels are therefore among the places that take inserts.

Temperature for Acetal

DuPont runs the nozzle and hot runner at 190 °C (374 °F) for Delrin. A skin of melt stays still against the metal wall there. Higher settings degrade it after a few hours and call for more frequent cleaning. A hot runner that last ran a flame-retardant or PVC grade is cleaned before acetal runs in it.

Dead Spots and Color

The still skin is why a color change drags out over many shots. To find dead spots, DuPont changes color and molds 10 minutes without a break. The system is then taken apart, and the places still holding the first color are where degraded resin will later be released.

Mold Maintenance and Spare Inserts Across a Bridge Injection Molding Run

How a bridge mold is cleaned, inspected and fitted with inserts across a run, so that wear is recorded, predicted and met with spares instead of stoppages.

What a Bridge Mold Needs Between LotsThe aluminum maintenance column is plain on the first rule: an aluminum mold is taken apart and cleaned thoroughly after every run of parts, and cleaned again before storage, however short the run. It can often run five to seven days before it needs cleaning, the author notes, though some resins and some molds with actions need it after two to three days.

Color Matching Molded Parts With Masterbatch in a Production Run

How masterbatch color is matched, dosed, distributed and measured so that every lot of a molded part matches the standard agreed at the first article.

How Masterbatch Color Is Held Across a RunThree things have to stay constant for color to hold. The masterbatch has to be the same formulation at the same let-down ratio, the melt has to distribute it evenly, and the part has to be measured the same way each time.

Short Shot, Sink and Flash in Injection Molding Traced to Their Cause

Short shots, sinks and flash traced to the melt volume, pressure and steel behind them, with the checks that find the cause before a setting is moved.

What Short Shots, Sink and Flash Have in CommonA short shot is a part the cavity never finished. BASF's troubleshooting brochure for engineering thermoplastics describes it as a part not completely formed, mainly in the areas furthest from the gate or in thin walls.

Gate Location and Gate Freeze in Injection Molding

Where a gate goes, how big it is and how long it stays open, with the weight study that sets hold time from the gate itself.

How Gate Location and Gate Freeze Shape a Molded PartAutodesk's Moldflow design rules open with the claim that gate position strongly affects material orientation and warpage, and that changing the gate is sometimes the only way to control orientation. Every gate injects under the same pressure, and the aim of gating is to avoid overpacking some paths while others are still filling, because unequal packing gives unequal shrinkage.

How Many Parts One Aluminum Injection Mold Gives

A mold's life is a toolmaker's rating for a stated resin and cavity count, converted into parts per tool and then into tools per quantity.

What Sets the Number of Parts One Aluminum Mold GivesThree things set it, and they act together. One is the alloy and where in the plate the cavity sits.

Cycle Time and Parts per Hour in a Bridge Injection Molding Run

A cycle is the sum of fill, hold, cooling and press motions, and a supplier's number is only as good as the pack and cooling times behind it.

What Sets Cycle Time and Parts per HourA molding cycle is a loop of seven moves: the mold closes, the cavity fills, the pack and hold phase runs, the part cools, the mold opens, the part is ejected, and the screw recovers for the next shot. Recovery runs while the part cools, which is why DuPont's nylon guide asks for screw speeds adjusted so that screw retraction time is shorter than the cooling phase.

How to Start Up an Injection Mold and Take the First Shots

A new mold is started cold on purpose, filled in stages with short shots, and read for vents, gates and heat before any process is fixed.

The Start-Up Sequence from a Cold Barrel to the First ShotEight moves take a machine from cold to its first complete part. The first four prepare the melt, the next three shape the shot, and the last one is a decision: whether the part describes the tool or only the settings.

Drying Resin and Setting Melt Temperature Before the First Injection Molded Part

Pellets are dried to a measured moisture limit, held there to the hopper, and melted inside a window that the resin maker prints.

What Dry Resin and a Correct Melt Temperature ProtectWater in a nylon melt is not a surface problem. DuPont explains that water carried into the melt triggers hydrolysis, which breaks the polymer down, costs toughness and strength, and makes the melt flow more easily.

Acetal Homopolymer Injection Molding Properties and Gate Rules

Delrin 500P read from the maker's sheet and molding tips: why acetal shrinks and needs a packed gate, how hot the melt may run, and what to check on an aluminum tool.

Delrin 500P Properties in Metric and Inch UnitsDelrin 500P NC010 is a medium-viscosity acetal homopolymer, and Delrin prints its ISO values as the reference beside 500CPE on its own product data sheet. The grade has a melt mass-flow rate of 15 g/10 min at 190 °C and 2.16 kg under ISO 1133.

Request an Injection Molding Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Injection Molding chosen.

Request a Quote