Gate Land

The gate land is the short length of the gate, under 1 mm (0.04 in) in nylon, whose length decides when the gate freezes.

Every Gate Land article of the Injection Molding Resources, newest first, each written from published standards, research and makers’ data.

Meaning

The gate land is the short length of the gate, under 1 mm (0.04 in) in nylon, whose length decides when the gate freezes. Its length decides how long the gate stays open during the hold phase. A long land freezes before the part is packed. A worn land changes the packing before anything else does.

Typical Range

DuPont’s nylon guide gives a gate land under 1 mm (0.04 in), with gate thickness at 50 to 75 percent of the part. The Delrin tips set a tunnel gate length under 0.8 mm (0.03 in) for acetal, so the gate does not freeze early. On a 4 mm (0.16 in) acetal wall that means a gate diameter of at least 2 mm and a land shorter than 0.8 mm.
Read More

Wear

The land sits at the point of highest flow and shear in the cavity, so it is the first place to wear. When it wears larger, the packing changes and the part can turn heavier or lighter. A part weight study repeated during a run reads that change before the cavity shows damage. Where an abrasive resin runs in aluminum, a hardened steel gate insert can carry the land.

Inspection

An acetal gate land of 0.8 mm at most is a precise feature. It is checked at each cleaning of the tool. The check sits beside an agreed hold pressure limit for an aluminum tool.

Order Wording

An acetal order can name the tunnel gate within its four criteria and a land length of at most 0.8 mm. That wording ties the dimension result to a gate that can be inspected.

Gate Location and Gate Freeze in Injection Molding

Where a gate goes, how big it is and how long it stays open, with the weight study that sets hold time from the gate itself.

How Gate Location and Gate Freeze Shape a Molded PartAutodesk's Moldflow design rules open with the claim that gate position strongly affects material orientation and warpage, and that changing the gate is sometimes the only way to control orientation. Every gate injects under the same pressure, and the aim of gating is to avoid overpacking some paths while others are still filling, because unequal packing gives unequal shrinkage.

How Many Parts One Aluminum Injection Mold Gives

A mold's life is a toolmaker's rating for a stated resin and cavity count, converted into parts per tool and then into tools per quantity.

What Sets the Number of Parts One Aluminum Mold GivesThree things set it, and they act together. One is the alloy and where in the plate the cavity sits.

How to Start Up an Injection Mold and Take the First Shots

A new mold is started cold on purpose, filled in stages with short shots, and read for vents, gates and heat before any process is fixed.

The Start-Up Sequence from a Cold Barrel to the First ShotEight moves take a machine from cold to its first complete part. The first four prepare the melt, the next three shape the shot, and the last one is a decision: whether the part describes the tool or only the settings.

How Tightly Acetal Parts Hold Dimension in Injection Molding

Acetal dimension spread measured on one part under four press settings, with the gate and cooling rules behind it and a tolerance budget for a 50 mm feature.

Outer Diameter Spread Under Four Packing and Cooling SettingsThe test part in DuPont's tips is a tribological sample used for wear and friction testing, a part whose outer diameter has to be as dimensionally precise as possible. DuPont molded it under four settings, measured the outer diameter and reported the mean with its variation.

Acetal Homopolymer Injection Molding Properties and Gate Rules

Delrin 500P read from the maker's sheet and molding tips: why acetal shrinks and needs a packed gate, how hot the melt may run, and what to check on an aluminum tool.

Delrin 500P Properties in Metric and Inch UnitsDelrin 500P NC010 is a medium-viscosity acetal homopolymer, and Delrin prints its ISO values as the reference beside 500CPE on its own product data sheet. The grade has a melt mass-flow rate of 15 g/10 min at 190 °C and 2.16 kg under ISO 1133.

Request an Injection Molding Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Injection Molding chosen.

Request a Quote