CavityPart WeightBarrel

How Many Parts One Aluminum Injection Mold Gives

A mold's life is a toolmaker's rating for a stated resin and cavity count, converted into parts per tool and then into tools per quantity.

An opened aluminum injection mold half with a polished cavity, a row of molded black parts in front of it.

Alloy 7075-T651 plate carries a yield strength of 517 MPa (75 ksi) at 25 mm (1 in) thick and 221 MPa (32 ksi) at 254 mm (10 in) thick, according to the thyssenkrupp mold materials table. The same alloy, bought from the same mill, is less than half as strong in the middle of a thick block as at the surface of a thin one. A mold cavity cut into that block inherits the number, and so does the count of parts it will mold.

There is no single count of parts an aluminum mold gives, and the makers’ own documents do not print one. What exists is a set of physical drivers, each with a published figure: the hardness and strength of the alloy, the abrasiveness of the resin, the places where steel has to take over, and the heat the tool is cycled through. This piece lays those drivers out, shows how a toolmaker’s rated life becomes parts per tool and tools per quantity, and lists the questions a buyer should have answered in writing before the quantity is committed.

What Sets the Number of Parts One Aluminum Mold Gives

Three things set it, and they act together. One is the alloy and where in the plate the cavity sits. Another is what flows over the cavity surface, the resin and its filler. The last is how the tool is built around the cavity: which parts are aluminum, which are hardened steel or copper alloy, and how it is held and heated.

Rated life is the toolmaker’s statement of the expected count, and it is a design target, not a measured result for the part in question. Toolmakers rate a tool from experience with similar parts, resins and alloys. A buyer who asks for the rating also asks which resin and which cavity count it assumes, because the same tool can have a different rating for an unfilled resin than for a glass-filled one.

The count is then turned into parts through the cavity count. One cavity gives one part per shot and four cavities four, so parts per tool is cavities multiplied by shots, minus the shots spent on setup and scrap. More cavities reach a quantity in fewer shots, and each cavity wears with every shot, so the arithmetic favors more cavities only until the machine and the part geometry set a limit.

The number printed in a quote is a shots figure for a stated resin and a stated cavity count. Convert it into parts per tool before comparing one quote with another.

Aluminum Alloys and Tool Steels Compared by Hardness and Strength

Hardness and yield strength are the plainest published measures of how a cavity surface resists the plastic flowing over it and the clamp pressing it shut. Table 1 collects what thyssenkrupp Materials NA prints for the mold materials in common use, with yield strength converted to MPa.

Table 1. Hardness and yield strength of mold materials, from thyssenkrupp Materials NA
Material Hardness as printed Yield strength at 25 mm (1 in) plate Yield strength at thickest size listed
QC-10 aluminum 170 to 150 HB by thickness 538 MPa (78 ksi) 448 MPa (65 ksi) at 508 mm (20 in)
Alumold 500 aluminum 175 to 150 HB by thickness 538 MPa (78 ksi) 414 MPa (60 ksi) at 508 mm (20 in)
7075-T651 aluminum 150 HB 517 MPa (75 ksi) 221 MPa (32 ksi) at 254 mm (10 in)
6061-T651 aluminum 95 HB 290 MPa (42 ksi) 269 MPa (39 ksi) at 254 mm (10 in)
P-20 steel 26 to 34 HRC 896 MPa (130 ksi) Not listed by thickness
H-13 steel 50 to 54 HRC 1,172 MPa (170 ksi) Not listed by thickness
S-7 steel 55 to 62 HRC 1,586 MPa (230 ksi) Not listed by thickness

Two readings stand out. A QC-10 plate keeps most of its strength through thickness, while 7075 does not. The table’s description calls QC-10 a very high-strength mold plate with very low quench sensitivity and uniform hardness through thickness up to 24 in, and it calls 7075-T651 a quench-sensitive alloy whose thicker sections vary through the thickness. A toolmaker choosing a plate for a deep cavity is choosing between those two behaviors.

The second reading is the gap between aluminum and steel. Hardened steel sits at 50 HRC and above, while P-20 prehardened steel at 26 to 34 HRC has a yield strength near 896 MPa (130 ksi), about two thirds above a QC-10 plate. MoldMAX’s brochure puts the aluminum alloys on a different scale, Rockwell B, giving QC-10 B90 and Alumold B88 against 30 HRC for P-20 and 45 to 50 HRC for H-13. The scales cannot be compared digit for digit, but the ranking is unambiguous: aluminum is the softest cavity material in the table and tool steel the hardest.

A softer cavity wears and dents more easily. It also machines far faster and can be recut, welded and corrected, which is the reason a bridge tool is made of it. The same softness that shortens the life of a tool lengthens the list of changes that can be made to it after the first shots. An aluminum tool is itself machined aluminum milled from plate in a fraction of the time a hardened steel cavity takes, which is the reason a bridge tool reaches its first shots sooner and also why it wears sooner.

Where Wear Starts in a Tool

Wear does not spread evenly over a mold. It starts where flow is fastest, where steel closes on steel, and where a part is pulled off the metal.

Resin filler is the first cause. DuPont’s nylon guide warns that glass-reinforced resins wear the barrel, screw and mold in places, and that large quantities call for precautions to protect the equipment. Its numbers concern the injection unit: specially treated bi-metallic barrels, screws and check rings last 5 to 10 times as long as standard ones. Molds get less attention in that passage, but the principle is the same, and the area around the gate sees the highest flow rate and shear of any region of the cavity.

The gate and its approach are the places to look first. DuPont gives the gate land length as under 1 mm (0.04 in) for nylons, and a short land sits right at the point of highest wear. When a gate wears larger, the packing behavior of the part changes, so a mold can start to give a heavier or a lighter part before its cavity shows any visible damage. A part weight study becomes a wear gauge when it is repeated during a run.

Hot runner contact points are the second place. Arconic’s fact sheet puts hardened steel inserts, sleeves, bushings or pads wherever the hot runner touches aluminum, to isolate heat and to protect the base block from wear. The inserts also have to be hard and strong enough to resist hobbing from the thrust pads, support ring, nozzle head, nozzle tip and inlet area. Water-cooled gate inserts go with blind nozzle tips.

Aluminum is rarely worn out everywhere at once. A tool usually ends at a gate, a shut-off or a thin steel-to-aluminum interface, and each of those can be built as a replaceable steel part.

Heat, Expansion and the Thermal Life of the Tool

A mold is heated and cooled thousands of times, and each cycle moves its dimensions. Aluminum expands at about twice the rate of P-20 steel: 24.7 × 10⁻⁶ per K (13.7 × 10⁻⁶ per °F) for QC-10 against 12.2 × 10⁻⁶ per K (6.8 × 10⁻⁶ per °F), and Arconic’s sheet and thyssenkrupp’s table agree on it. A plate 300 mm long that changes by 40 K grows about 0.30 mm in QC-10 and about 0.15 mm in P-20, by simple multiplication of those coefficients.

That is the arithmetic behind the fact sheet’s instruction to account for expansion in the mold and hot runner design. A hot runner manifold in steel mounted into an aluminum plate does not stay aligned over a temperature swing unless the fixing, the dowels and the clearances are designed for it. Location and expansion dowels are listed in the sheet among the places where inserts are needed.

High temperature affects the alloys themselves. The thyssenkrupp descriptions single out Weldural and 2024-T351 for coping with long exposure to heat better than most heat treated aluminum alloys, and they rank 6061-T651 high for conductivity but low for strength and surface hardness, which rules it out where those matter. Resin choice thus sets the thermal duty of the tool through mold temperature, and DuPont’s reinforced nylons at 100 to 120 °C (210 to 250 °F) are a harder duty than a polycarbonate at 65 to 82 °C (150 to 180 °F).

Conductivity works for the tool as well. QC-10 conducts at 159 W/mK (92 Btu/ft/hr/°F) against 29 W/mK (17) for P-20, so heat moves through an aluminum plate far more readily.

Steel Inserts and Copper Alloys in an Aluminum Tool

The way to extend an aluminum tool is to put the highest wear and highest heat into other metals. Three kinds of insert are in published use.

  • Hardened steel in gate areas, shut-offs and hot runner contact points, as Arconic specifies for QC-10 molds.
  • Beryllium copper cores, pins and inserts in areas that need heat taken out fast. thyssenkrupp lists MoldMAX alloys for whole molds or as inserts in steel or aluminum molds, and the MoldMAX brochure positions them as the core material working with steel bases and cavities.
  • Copper alloy inserts at spots where a part sticks. Covestro’s polycarbonate sheet suggests beryllium copper for ribs, deep cores and other areas where sticking is likely.

Each of these is a decision about the tool’s end of life. If the gate insert can be swapped, the tool outlasts the gate. Make the core pin a replaceable copper alloy part, and the tool does not have to be recut for a worn pin.

The MoldMAX brochure carries a safety note that belongs with any copper beryllium insert. Solid metal is not a special risk to handle, yet airborne beryllium can harm health when the recommended handling practices are skipped, and the Safety Data Sheet is read before work starts. A buyer does not handle the inserts, but a toolmaker can reasonably be asked to confirm that those practices are followed.

From Rated Shots to Parts per Tool and Tools per Quantity

A buyer asks for a quantity, and the tool is rated in shots, so a conversion sits between them. Four terms go into it, and each should appear in the quote or the toolmaker’s letter.

Table 2. The terms that turn a rated life into tools per quantity
Term What it is Where it comes from
Rated shots The toolmaker’s expected life for a stated resin Toolmaker’s written rating
Cavities Parts per shot Tool design
Setup and scrap shots Shots spent in trials, T1 samples and startup Mold trial record
Quantity Parts the buyer wants in total Purchase order

The conversion is then direct. Parts per tool are cavities multiplied by usable shots, where usable shots are the rated shots less the setup and scrap shots. Tools per quantity are the quantity divided by parts per tool, rounded up. Any figure written in a quote that is not tied to a resin and a cavity count cannot go into that formula.

Quantity enters in a second way, through batches. A bridge run is often made in lots, with the tool left at rest between them, and each restart spends a few setup shots and a short drying and purging sequence. Splitting the quantity into more lots spends more shots without adding parts, and the toolmaker’s rated life has to cover them.

Wear is not linear. A tool can mold good parts for most of its life and then drift in a short stretch, so the useful count is the count at which parts remain inside the drawing, not the count at which the cavity fails. Toolmakers may rate by either measure, and the buyer should ask which.

Ask for the rated life, the resin it assumes, the cavity count and the parts that count covers. A shots number without those four is not a quote.

Steel is not always the alternative. DuPont’s Delrin sheet advises correcting the cavity only after the gate and the process have been checked, and an aluminum tool makes that last step cheap. A tool that can be recut after a trial is a tool whose first shots are still useful design information, and that is worth more in a bridge run than a long rated life on a cavity that was never adjusted.

Signs That a Tool Is Nearing the End

A tool gives notice in advance, and a buyer who reads the first article report and the run records can see it. Four signs are common.

  • Part weight drifts at a hold time that used to give a plateau, which points to a gate, a shut-off or a check ring that has changed.
  • Flash appears at a parting line or an ejector pin that was clean in the first shots.
  • Burn marks appear at the end of flow, because vents have clogged or deposits have formed.
  • A dimension moves in one direction across successive lots, as a cavity or a core wears away.

Resin deposits are also a cause. DuPont’s Delrin sheet notes that a resin which foams when molten can quickly cause mold deposit, so a deposit is a process symptom as much as a wear symptom. The resin and dryer records from the lot give the answer, and a worn tool is only one of the causes.

None of the signs needs a new tool in itself. Aluminum can be recut, a gate insert replaced or a vent cleaned, and DuPont’s best-practice list for a part out of tolerance ends with checking the gate and process conditions first and correcting the cavity only after that. The sequence is worth keeping, because a repair made to the wrong thing consumes shots in the tool’s rated life.

When the Next Tool Is the Right Decision

The next tool is justified by a condition that can be seen in the records, not by a calendar date. Four conditions recur.

  1. The remaining quantity, divided by the parts per tool, is more than one more tool.
  2. The resin has changed to a filled grade, and the rating that applied to the unfilled grade no longer holds.
  3. Cycle time has become the main variable in the program, and a tool with a faster-cooling alloy would change it. MoldMAX claims its alloys cut cycle time by 15 to 50 % through conductivity up to ten times that of tool steel, and the figure is the maker’s.
  4. The geometry has settled, because a steel cavity cannot be reworked as easily as aluminum.

The last condition is the one most often missed. A bridge tool is cut in aluminum or soft steel because it can be corrected, so the design should be frozen before a tool is cut that cannot. The records from the aluminum tool, the weight study, the cooling trials and the dimensions, go to the next toolmaker as a starting point. A supplier of low-volume injection molding can state those records and the rated life together, and that is the basis on which bridge production quantities are planned in tools, not hopes.

Sources and Further Reading

Request an Injection Molding Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Injection Molding chosen.

Request a Quote