Dry as Molded

Dry as molded is the state of a nylon part or specimen fresh from the press, before it takes up water from the air.

Every Dry as Molded article of the Injection Molding Resources, newest first, each written from published standards, research and makers’ data.

Meaning

Dry as molded is the state of a nylon part or specimen fresh from the press, before it takes up water from the air. Datasheets print a dry column beside a conditioned one. The two describe different parts. A drawing names which state a dimension or property refers to.

Datasheet Columns

The Zytel 70G33HS1L glass nylon sheet reads 11,000 MPa (1.60 million psi) tensile modulus dry as molded. Conditioned, the same bar reads 8,000 MPa (1.16 million psi). Tensile stress at break falls from 200 to 140 MPa, and flexural modulus from 9,500 to 6,000 MPa. Strain at break rises from 3.5 to 5.0 percent.
Read More

Shrinkage Figure

DuPont measures nylon mold shrinkage at 23 °C in the dry-as-molded state, after 24 to 48 hours at 23 °C and 50 percent relative humidity. For nylon, the ISO 294-4 value therefore describes the dry state only. A part that later absorbs 1.8 percent water swells beyond that figure.

Uptake After Molding

A part ejected dry as molded starts absorbing water at once, at a rate set by its thickest wall. DuPont’s guide plots the uptake over 300 days for walls of 1.5, 3.2 and 6.4 mm. A measurement taken soon after molding sits at the shrunken, dry dimension. DuPont’s ceiling of 0.2 percent water before molding is why a part leaves the press nearly dry.

Impact

DuPont’s notched impact charts for nylon are labeled dry as molded. Impact strength climbs with ambient humidity and temperature. A test taken dry as molded and one taken after conditioning describe different parts, and the inspection plan says which one governs.

How Temperature Changes the Size of a Molded Plastic Part at the Gauge

How coefficients of expansion turn a few degrees of gauge temperature into hundredths of a millimeter, by resin and direction, and what a drawing should state.

Linear Thermal Expansion of Polycarbonate, Glass-Filled Nylon and AcetalLinear thermal expansion is reported on datasheets as a coefficient, the length change per unit length per degree. The three makers print it by the ISO or TMA method, and they differ in how finely they split it.

Injection Molding Shrinkage Along and Across the Flow by Material

Molding shrinkage read by direction and condition for three resins, with the process settings that move it and the way a first sample turns it into a cavity allowance.

Shrinkage of Polycarbonate, Glass-Filled Nylon 66 and Acetal Along and Across the FlowISO 294-4:2018 sets out the method for measuring mold shrinkage and post-mold shrinkage of injection molded thermoplastic test specimens, parallel and normal to the direction of melt flow. Resin makers print the result in two lines, one per direction.

Glass-Filled Nylon 66 in Injection Molding and What It Does to an Aluminum Tool

How a glass-reinforced nylon behaves dry and conditioned, in the press and on an aluminum tool, and what its datasheet leaves for the buyer to settle.

Properties of 30 Percent Glass-Filled Nylon 66 Dry and ConditionedPA66 with 30 percent glass is one of the most common reinforced engineering grades, and BASF's Ultramid A3WG6 LT BK, a laser-transparent black grade whose sheet is dated 09/2026, is a clear example of how the family reads. The sheet names the polymer PA66-GF30 and gives its typical values for uncolored product at 23 °C.

Request an Injection Molding Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Injection Molding chosen.

Request a Quote