Process settings are the values a press runs a part at: melt and mold temperature, fill time, transfer position, hold and cooling.

Every Process Settings article of the Injection Molding Resources, newest first, each written from published standards, research and makers’ data.

Meaning

Process settings are the values a press runs a part at: melt and mold temperature, fill time, transfer position, hold and cooling. Written on a settings sheet, they are what makes one lot repeat another. A dimension depends on them as much as on the cavity. A measurement report without them cannot show why a part is the size it is.

Effect on Size

DuPont’s nylon guide shows settings moving shrinkage. Hold pressure lowers it by about 0.1 percent for each 10 MPa (1,450 psi). Hold time to the weight plateau brings it to its minimum. A hotter mold raises it and a thicker wall raises it. A production part molded at its own best settings is not the plaque behind the printed number.
Read More

Correction Order

DuPont’s Delrin tips put gate design and process settings first when a part misses its tolerance. The cavity is corrected only after that. The tips close with the advice to leave the process settings alone in the chase for dimensional precision or consistency. Settings that cannot be repeated give a first article the lot cannot match.

Sign-Off

A change in resin grade, color or process settings after sign-off reopens the dimensions it affects. The corrected conditions go on the setup sheet, so the production run repeats them. A buyer keeps the settings sheet with the first-article report and compares each later lot with it.

Surface

Settings bear on the finish as well. Covestro’s sheet gives the vent depth and the mold temperature range among the settings that touch the surface of a clear part.

Injection Molding Shrinkage Along and Across the Flow by Material

Molding shrinkage read by direction and condition for three resins, with the process settings that move it and the way a first sample turns it into a cavity allowance.

Shrinkage of Polycarbonate, Glass-Filled Nylon 66 and Acetal Along and Across the FlowISO 294-4:2018 sets out the method for measuring mold shrinkage and post-mold shrinkage of injection molded thermoplastic test specimens, parallel and normal to the direction of melt flow. Resin makers print the result in two lines, one per direction.

SPI Mold Finish Grades A-1 to D-3 for Injection Molded Parts

The SPI finish grades read for a buyer, with what each method gives, how texture costs draft, and how a finish is written and kept on an aluminum tool.

What the Twelve SPI Finish Grades SpecifyThe SPI system names a finish by a letter and a number. Its letter gives the finishing method, A for diamond buff, B for grit paper, C for stone and D for dry blast, while the number runs from 1, the finest within a letter, to 3, the coarsest.

ISO 20457 Tolerances for Plastic Molded Parts Read for the Buyer

How ISO 20457 is worded for plastic molded parts, what a supplier signs when a drawing cites it, and which items stay outside it for the order to settle.

What ISO 20457 Covers for Injection Molded PartsAccording to the abstract published by the Swedish Institute for Standards (SIS), ISO 20457 specifies possible manufacturing tolerances for plastic moulded parts, and it covers all integral features with general tolerances, using a surface profile tolerance within a specified datum system. It applies to injection moulding, injection compression moulding, transfer moulding, compression moulding and rotational moulding of non-porous parts in thermoplastics, thermoplastic elastomers and thermosets.

Request an Injection Molding Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Injection Molding chosen.

Request a Quote