Shot Size

Shot size is the amount of melt a press injects per cycle, judged against the barrel's capacity and the screw's diameter.

Every Shot Size article of the Injection Molding Resources, newest first, each written from published standards, research and makers’ data.

Meaning

Shot size is the amount of melt a press injects per cycle, judged against the barrel’s capacity and the screw’s diameter. Too small a shot keeps resin in the barrel for many cycles. Too large a shot cannot be melted fast enough for the cycle. Both limits sit in the maker’s data sheet.

Barrel Share

On Makrolon 2407 the shot fills 30 to 70 percent of the cylinder. Covestro’s conductive grades ask for a shot stroke of 2 to 3 screw diameters. Both keep heat exposure from degrading the base resin. DuPont warns against a machine size or screw diameter that gives a shot weight too low.
Read More

Press Data

ARBURG’s ALLROUNDER 370 A, a 600 kN (65 ton) electric press, lists three injection units. At the larger screw of each, the maximum polystyrene shot is 65, 105 and 172 g (2.3, 3.7 and 6.1 oz). The smaller screws cut it to 29, 54 and 97 g (1.0, 1.9 and 3.4 oz). A small part in the 290 unit leaves most of the barrel full of resin that is waiting.

Throughput

A shot of 30 g at a 26 second cycle is 138 shots an hour, about 4.2 kg/h (9.1 lb/h). In PA 6.6 the 20 mm screw tops out at 2.8 kg/h and cannot keep that cycle. The 30 mm screw of the same unit, at 4.9 kg/h, has only a thin margin. The press fits the part when its throughput covers the cycle and its shot turns the barrel over.

Long Residence

Material that sits about an hour at molding temperature builds residue on the screw flights and check ring. The screw can seize and has to be pulled and cleaned.

Polypropylene for Living Hinges in Injection Molding

Polypropylene for living hinges read from design guides and molding columns: grade choice, hinge dimensions, gating across the web, cooling and the tests that prove a hinge.

Why Polypropylene Makes a Living HingeThe MIT design note explains the mechanism. When a partly oriented polypropylene web is cold drawn on its first flex, it stretches by ratios of 2 or 3 to 1, and its tensile strength rises sharply.

ABS and PC/ABS Blends in Injection Molding

ABS and PC/ABS read from the makers' datasheets: drying, processing windows, shrinkage, snap-fit strain, impact and when the blend earns its stricter dryer.

How ABS and PC/ABS Differ in Injection MoldingABS is a terpolymer, and Moldflow's material page describes its structure: a continuous phase of styrene-acrylonitrile with a dispersed phase of polybutadiene rubber. Acrylonitrile brings hardness and chemical and heat resistance, styrene brings processability, gloss and strength, and butadiene brings toughness and impact strength.

Cycle Time and Parts per Hour in a Bridge Injection Molding Run

A cycle is the sum of fill, hold, cooling and press motions, and a supplier's number is only as good as the pack and cooling times behind it.

What Sets Cycle Time and Parts per HourA molding cycle is a loop of seven moves: the mold closes, the cavity fills, the pack and hold phase runs, the part cools, the mold opens, the part is ejected, and the screw recovers for the next shot. Recovery runs while the part cools, which is why DuPont's nylon guide asks for screw speeds adjusted so that screw retraction time is shorter than the cooling phase.

Drying Resin and Setting Melt Temperature Before the First Injection Molded Part

Pellets are dried to a measured moisture limit, held there to the hopper, and melted inside a window that the resin maker prints.

What Dry Resin and a Correct Melt Temperature ProtectWater in a nylon melt is not a surface problem. DuPont explains that water carried into the melt triggers hydrolysis, which breaks the polymer down, costs toughness and strength, and makes the melt flow more easily.

Polycarbonate Injection Molding Properties for Clear and Tough Parts

Polycarbonate read from the maker's sheets for a buyer: what it molds like when dry and hot, how thin walls fill, and what to ask of an aluminum tool.

Makrolon 2407 Properties in Metric and Inch UnitsMakrolon 2407 is a low-viscosity, general-purpose, UV-stabilized, easy-release polycarbonate with a melt volume-flow rate of 19 cm³/10 min at 300 °C and 1.2 kg under ISO 1133. Its ISO short name is ISO 7391-PC,MLR,(,,)-18-9.

Request an Injection Molding Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Injection Molding chosen.

Request a Quote