Tensile Modulus

Tensile modulus is a plastic's short-term stiffness in tension, measured on a molded bar under ISO 527 and printed in MPa. It is the headline stiffness on a datasheet.

Every Tensile Modulus article of the Injection Molding Resources, newest first, each written from published standards, research and makers’ data.

Meaning

Tensile modulus is a plastic’s short-term stiffness in tension, measured on a molded bar under ISO 527 and printed in MPa. It is the headline stiffness on a datasheet. It is taken at 23 °C in about a minute of loading. A part loaded for months or kept wet keeps less of it.

Values

Delrin 500P acetal reads 3,100 MPa (450,000 psi). Makrolon 2407 polycarbonate reads 2,400 MPa (348,000 psi). Zytel 70G33HS1L glass nylon reads 11,000 MPa (1.60 million psi) dry as molded. Covestro measures its value under ISO 527-1 and -2 at 23 °C and 50 percent relative humidity.
Read More

Moisture

The glass nylon bar reads 8,000 MPa (1.16 million psi) once conditioned in room air. That gap of 27 percent is the first thing a buyer reads before drawing a part in this resin. Glass fibers carry the stiffness, and the polymer between them softens as it takes up water.

Creep Effect

Short-term modulus overstates what a loaded part keeps. Acetal’s creep modulus at 1,000 hours is 1,600 MPa against its 3,100 MPa short-term figure. A clip that stays deflected for months loads the material in creep and relaxes if it was designed on the short-term number.

Temperature

The Zytel sheet’s stress-strain and secant modulus curves run from -40 to 149 °C (-40 to 300 °F). Stiffness falls along them as the part warms. A test at 23 °C says little about a part that runs at 80 °C.

Interpretation

A drawing that quotes a modulus quotes it with its state, dry or conditioned, and its time base.

ABS and PC/ABS Blends in Injection Molding

ABS and PC/ABS read from the makers' datasheets: drying, processing windows, shrinkage, snap-fit strain, impact and when the blend earns its stricter dryer.

How ABS and PC/ABS Differ in Injection MoldingABS is a terpolymer, and Moldflow's material page describes its structure: a continuous phase of styrene-acrylonitrile with a dispersed phase of polybutadiene rubber. Acrylonitrile brings hardness and chemical and heat resistance, styrene brings processability, gloss and strength, and butadiene brings toughness and impact strength.

Polycarbonate Injection Molding Properties for Clear and Tough Parts

Polycarbonate read from the maker's sheets for a buyer: what it molds like when dry and hot, how thin walls fill, and what to ask of an aluminum tool.

Makrolon 2407 Properties in Metric and Inch UnitsMakrolon 2407 is a low-viscosity, general-purpose, UV-stabilized, easy-release polycarbonate with a melt volume-flow rate of 19 cm³/10 min at 300 °C and 1.2 kg under ISO 1133. Its ISO short name is ISO 7391-PC,MLR,(,,)-18-9.

Glass-Filled Nylon 66 in Injection Molding and What It Does to an Aluminum Tool

How a glass-reinforced nylon behaves dry and conditioned, in the press and on an aluminum tool, and what its datasheet leaves for the buyer to settle.

Properties of 30 Percent Glass-Filled Nylon 66 Dry and ConditionedPA66 with 30 percent glass is one of the most common reinforced engineering grades, and BASF's Ultramid A3WG6 LT BK, a laser-transparent black grade whose sheet is dated 09/2026, is a clear example of how the family reads. The sheet names the polymer PA66-GF30 and gives its typical values for uncolored product at 23 °C.

Acetal Homopolymer Injection Molding Properties and Gate Rules

Delrin 500P read from the maker's sheet and molding tips: why acetal shrinks and needs a packed gate, how hot the melt may run, and what to check on an aluminum tool.

Delrin 500P Properties in Metric and Inch UnitsDelrin 500P NC010 is a medium-viscosity acetal homopolymer, and Delrin prints its ISO values as the reference beside 500CPE on its own product data sheet. The grade has a melt mass-flow rate of 15 g/10 min at 190 °C and 2.16 kg under ISO 1133.

Request an Injection Molding Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Injection Molding chosen.

Request a Quote