Hold Pressure

Hold pressure is the pressure the screw keeps on the melt after the cavity fills, feeding the part as it shrinks until the gate freezes.

Every Hold Pressure article of the Injection Molding Resources, newest first, each written from published standards, research and makers’ data.

Meaning

Hold pressure is the pressure the screw keeps on the melt after the cavity fills, feeding the part as it shrinks until the gate freezes. It sets how much plastic the part finally holds. That in turn sets the part’s weight, its shrinkage and much of its size. Resin makers print a range for it beside the melt and mold temperatures.

Typical Range

DuPont applies the highest possible hold pressure on nylon to reduce mold shrinkage, usually around 90 MPa (13,050 psi). The Zytel 70G33HS1L sheet gives 50 to 100 MPa (7,250 to 14,500 psi). Delrin 500P acetal takes 80 to 100 MPa (11,600 to 14,500 psi). Covestro’s Makrolon 2407 plaques for shrinkage are held at 500 bar (50 MPa). A shrinkage figure is therefore tied to the hold pressure that produced it.
Read More

Effect on Shrinkage

DuPont states that a 10 MPa (1,450 psi) variation in hold pressure gives about 0.1 percent variation in shrinkage. On a 100 mm (3.94 in) dimension that is about 0.10 mm. A 20 MPa drift doubles it to about 0.20 mm, as a straight extension of the guide’s rule. On a 120 by 80 mm glass nylon cover, a 10 MPa change moves the length 0.12 mm and the width 0.08 mm. Those movements are larger than the tolerance a close-fitting lid would carry. DuPont’s charts for unreinforced nylon 66 show shrinkage falling as hold pressure rises. A process change and a thermometer can move a part by the same amount. On acetal, a gauge room 10 °C warm adds an error of the same order as a 10 MPa hold change. The same holds for glass nylon across the flow. A first-sample correction is only as good as the temperature of measurement behind it.

Hold Duration

Hold pressure acts only while the gate is open, so it is read together with hold time. The Delrin 500P sheet gives 8 s of hold per millimeter of wall, and the Zytel sheet gives 3 s per millimeter. On a 4 mm (0.16 in) acetal wall the sheet suggests 32 seconds as a first estimate. DuPont’s own acetal test part found its optimum at 15 seconds by weighing parts. The sheet figure is a start, and the weight plateau is the setting. The guide asks for a single pressure setting over the whole hold time. A changing pressure can leave non-uniform crystallinity in the part and lower its mechanical properties. A press that cannot hold pressure steady within a few MPa will not give a stable shrinkage, whatever the drawing says.

Failure Mode

A poor process fails the two resin families in opposite ways. An amorphous resin tends to be over-packed and shows flash and stress near the gate. A semi-crystalline resin tends to be under-packed and shows sink, voids and size. Both are read with the same weight study.

Press and Tool Limits

The press holds the mold shut against the pressure in the cavities. A rough ceiling is the clamp force divided by the pressure. A 600 kN (65 ton) press at 90 MPa holds about 6,700 mm² (10.3 in²) of projected area, runner included. Real cavity pressure falls below the pressure at the screw as melt flows through runner and gate. The ceiling is therefore an upper bound, and flow analysis gives the final figure. A hold pressure of up to 100 MPa is the upper end of what a steel production tool runs at. Whether an aluminum bridge tool is rated for it is a question for the toolmaker. The trade literature on aluminum tools warns that excessive injection pressure damages them through detail shifting and galling. An acetal or glass nylon order therefore carries an agreed pressure limit for the tool. The gate is checked at each cleaning, since a worn gate changes how the pressure reaches the part.

Record

Hold pressure goes on the setup sheet with the hold time found by weighing parts. A cycle quoted without its pack and hold settings cannot be checked against a weight study.

Short Shot, Sink and Flash in Injection Molding Traced to Their Cause

Short shots, sinks and flash traced to the melt volume, pressure and steel behind them, with the checks that find the cause before a setting is moved.

What Short Shots, Sink and Flash Have in CommonA short shot is a part the cavity never finished. BASF's troubleshooting brochure for engineering thermoplastics describes it as a part not completely formed, mainly in the areas furthest from the gate or in thin walls.

Gate Location and Gate Freeze in Injection Molding

Where a gate goes, how big it is and how long it stays open, with the weight study that sets hold time from the gate itself.

How Gate Location and Gate Freeze Shape a Molded PartAutodesk's Moldflow design rules open with the claim that gate position strongly affects material orientation and warpage, and that changing the gate is sometimes the only way to control orientation. Every gate injects under the same pressure, and the aim of gating is to avoid overpacking some paths while others are still filling, because unequal packing gives unequal shrinkage.

ABS and PC/ABS Blends in Injection Molding

ABS and PC/ABS read from the makers' datasheets: drying, processing windows, shrinkage, snap-fit strain, impact and when the blend earns its stricter dryer.

How ABS and PC/ABS Differ in Injection MoldingABS is a terpolymer, and Moldflow's material page describes its structure: a continuous phase of styrene-acrylonitrile with a dispersed phase of polybutadiene rubber. Acrylonitrile brings hardness and chemical and heat resistance, styrene brings processability, gloss and strength, and butadiene brings toughness and impact strength.

Cycle Time and Parts per Hour in a Bridge Injection Molding Run

A cycle is the sum of fill, hold, cooling and press motions, and a supplier's number is only as good as the pack and cooling times behind it.

What Sets Cycle Time and Parts per HourA molding cycle is a loop of seven moves: the mold closes, the cavity fills, the pack and hold phase runs, the part cools, the mold opens, the part is ejected, and the screw recovers for the next shot. Recovery runs while the part cools, which is why DuPont's nylon guide asks for screw speeds adjusted so that screw retraction time is shorter than the cooling phase.

How Temperature Changes the Size of a Molded Plastic Part at the Gauge

How coefficients of expansion turn a few degrees of gauge temperature into hundredths of a millimeter, by resin and direction, and what a drawing should state.

Linear Thermal Expansion of Polycarbonate, Glass-Filled Nylon and AcetalLinear thermal expansion is reported on datasheets as a coefficient, the length change per unit length per degree. The three makers print it by the ISO or TMA method, and they differ in how finely they split it.

Injection Molding Shrinkage Along and Across the Flow by Material

Molding shrinkage read by direction and condition for three resins, with the process settings that move it and the way a first sample turns it into a cavity allowance.

Shrinkage of Polycarbonate, Glass-Filled Nylon 66 and Acetal Along and Across the FlowISO 294-4:2018 sets out the method for measuring mold shrinkage and post-mold shrinkage of injection molded thermoplastic test specimens, parallel and normal to the direction of melt flow. Resin makers print the result in two lines, one per direction.

How Tightly Acetal Parts Hold Dimension in Injection Molding

Acetal dimension spread measured on one part under four press settings, with the gate and cooling rules behind it and a tolerance budget for a 50 mm feature.

Outer Diameter Spread Under Four Packing and Cooling SettingsThe test part in DuPont's tips is a tribological sample used for wear and friction testing, a part whose outer diameter has to be as dimensionally precise as possible. DuPont molded it under four settings, measured the outer diameter and reported the mean with its variation.

Glass-Filled Nylon 66 in Injection Molding and What It Does to an Aluminum Tool

How a glass-reinforced nylon behaves dry and conditioned, in the press and on an aluminum tool, and what its datasheet leaves for the buyer to settle.

Properties of 30 Percent Glass-Filled Nylon 66 Dry and ConditionedPA66 with 30 percent glass is one of the most common reinforced engineering grades, and BASF's Ultramid A3WG6 LT BK, a laser-transparent black grade whose sheet is dated 09/2026, is a clear example of how the family reads. The sheet names the polymer PA66-GF30 and gives its typical values for uncolored product at 23 °C.

Acetal Homopolymer Injection Molding Properties and Gate Rules

Delrin 500P read from the maker's sheet and molding tips: why acetal shrinks and needs a packed gate, how hot the melt may run, and what to check on an aluminum tool.

Delrin 500P Properties in Metric and Inch UnitsDelrin 500P NC010 is a medium-viscosity acetal homopolymer, and Delrin prints its ISO values as the reference beside 500CPE on its own product data sheet. The grade has a melt mass-flow rate of 15 g/10 min at 190 °C and 2.16 kg under ISO 1133.

Request an Injection Molding Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Injection Molding chosen.

Request a Quote