Drawing

The drawing is the 2D document that states a molded part's dimensions, tolerances and notes, and the conditions under which each is read.

Every Drawing article of the Injection Molding Resources, newest first, each written from published standards, research and makers’ data.

Meaning

The drawing is the 2D document that states a molded part’s dimensions, tolerances and notes, and the conditions under which each is read. For a molded part it carries more than geometry. It names the standard for general tolerances, the datum system, the finish of each face and the flame class at a wall. It also names the state a dimension is measured in.

Tolerance Note

A drawing that cites ISO 20457 names the edition by year, because the 2018 first edition is withdrawn and replaced by ISO 20457:2026. The title block says which features carry the general tolerance and which carry direct tolerances. The datum system is defined on the drawing, or proposed by the supplier and approved before the tool steel is cut. A tolerance written before the first sample is a hope, and one confirmed on it is a specification.
Read More

Measurement Condition

A dimensional tolerance travels with a measurement condition. A short note names the temperature, for example 23 ± 2 °C, and the moisture state for nylon. It names the time after molding, for example at least 24 hours, and any annealing. It names the instrument and the method. For a glass-filled grade it names the direction of the critical dimension relative to the gate. An annealed acetal dimension also states the annealing conditions and the time between annealing and measurement.

Finish Note

A finish note has four parts, the grade, the face, the texture and depth, and the reference. A display cover can read window face SPI A-2, side faces SPI C-1, no texture, approved sample plate as reference. Writing only high gloss leaves every part of that note open.

Flame Note

A drawing that says only flame retardant asks for no test at all. One that says UL 94 V-0 at 1.5 mm asks for one class at one thickness. Because a resin can change class with wall, the note says which wall it refers to.

Inspection Plan

For nylon, a test dry as molded and a test after conditioning describe different parts. The inspection plan says which one governs. Gate location and the flow direction belong on the drawing before the first sample, not in the inspector’s habits.

Color Matching Molded Parts With Masterbatch in a Production Run

How masterbatch color is matched, dosed, distributed and measured so that every lot of a molded part matches the standard agreed at the first article.

How Masterbatch Color Is Held Across a RunThree things have to stay constant for color to hold. The masterbatch has to be the same formulation at the same let-down ratio, the melt has to distribute it evenly, and the part has to be measured the same way each time.

Gate Location and Gate Freeze in Injection Molding

Where a gate goes, how big it is and how long it stays open, with the weight study that sets hold time from the gate itself.

How Gate Location and Gate Freeze Shape a Molded PartAutodesk's Moldflow design rules open with the claim that gate position strongly affects material orientation and warpage, and that changing the gate is sometimes the only way to control orientation. Every gate injects under the same pressure, and the aim of gating is to avoid overpacking some paths while others are still filling, because unequal packing gives unequal shrinkage.

Draft Angle by Texture Depth on Injection Molded Parts

How much draft a textured wall needs for its depth, under which conditions each published figure holds, and how the mold and the part are checked.

How Much Draft a Texture Depth NeedsStandex Engraving Mold-Tech's technical data sheet gives the current recommendation from the texture maker: 1° of draft for every 0.013 to 0.015 mm (0.0005 to 0.0006 in) of texture depth. Per 0.025 mm (0.001 in) that works out to between 1.7° and 2°.

IEC 60695-2-12 Glow Wire Flammability Index for Molded Parts

The glow wire flammability index read for a buyer: what IEC 60695-2-12 measures, how makers print it by thickness, and what a molded part's file can carry from it.

What IEC 60695-2-12 MeasuresThe scope, printed on the IEC webstore and in the 2021 preview, is short. The standard specifies the details of the glow wire test applied to specimens of solid electrical insulating materials, or other solid materials, to determine the glow wire flammability index, GWFI.

How Temperature Changes the Size of a Molded Plastic Part at the Gauge

How coefficients of expansion turn a few degrees of gauge temperature into hundredths of a millimeter, by resin and direction, and what a drawing should state.

Linear Thermal Expansion of Polycarbonate, Glass-Filled Nylon and AcetalLinear thermal expansion is reported on datasheets as a coefficient, the length change per unit length per degree. The three makers print it by the ISO or TMA method, and they differ in how finely they split it.

How Tightly Acetal Parts Hold Dimension in Injection Molding

Acetal dimension spread measured on one part under four press settings, with the gate and cooling rules behind it and a tolerance budget for a 50 mm feature.

Outer Diameter Spread Under Four Packing and Cooling SettingsThe test part in DuPont's tips is a tribological sample used for wear and friction testing, a part whose outer diameter has to be as dimensionally precise as possible. DuPont molded it under four settings, measured the outer diameter and reported the mean with its variation.

UL 94 Flammability Ratings Explained for Molded Plastic Parts

The UL 94 classes read as a buyer needs them: what each test does, how three common resin sheets print a rating, and what a supplier should show.

What UL 94 Measures and What It Is NotUL 94 is a family of small-scale flame tests on strips and plaques of plastic, run under laboratory conditions. UL's own page on combustion tests for plastics groups the classifications into twelve: HB, V-0, V-1 and V-2, 5VA and 5VB, VTM-0, VTM-1 and VTM-2, and HF-1, HF-2 and HBF for foams.

SPI Mold Finish Grades A-1 to D-3 for Injection Molded Parts

The SPI finish grades read for a buyer, with what each method gives, how texture costs draft, and how a finish is written and kept on an aluminum tool.

What the Twelve SPI Finish Grades SpecifyThe SPI system names a finish by a letter and a number. Its letter gives the finishing method, A for diamond buff, B for grit paper, C for stone and D for dry blast, while the number runs from 1, the finest within a letter, to 3, the coarsest.

ISO 20457 Tolerances for Plastic Molded Parts Read for the Buyer

How ISO 20457 is worded for plastic molded parts, what a supplier signs when a drawing cites it, and which items stay outside it for the order to settle.

What ISO 20457 Covers for Injection Molded PartsAccording to the abstract published by the Swedish Institute for Standards (SIS), ISO 20457 specifies possible manufacturing tolerances for plastic moulded parts, and it covers all integral features with general tolerances, using a surface profile tolerance within a specified datum system. It applies to injection moulding, injection compression moulding, transfer moulding, compression moulding and rotational moulding of non-porous parts in thermoplastics, thermoplastic elastomers and thermosets.

Request an Injection Molding Quote